Ad situs nostros interretiales salve!

Taenia metallica convertoris catalytici X8cral 20-6 pro elemento calefactori

Descriptio Brevis:


  • materia:faeces
  • forma:planum, fascia, folium
  • condicio:molliter recoctum
  • Detalia Producti

    Quaestiones Frequentes

    Etiquettae Productarum

    X8cral 20-6Folium Convertoris Catalytici

    Analysis Nominalis

    21.00 Cr, 6.00 Al, Bal. Fe

    Temperatura maxima continua operandi: 1250º C.

    Temperatura fusionis: 1500º C

    Crassitudo 0.05~0.1mm, latitudo 1-1000mm

    Usus: Conversores catalytici

    Materia 1.4767, DIN 17470

    Nomen marcae 1Cr13Al4 0Cr25Al5 0Cr21Al6 0Cr23Al5 0Cr21Al4 0Cr21Al6Nb 0Cr27Al7Mo2
    Compositio chemica principalis% Cr 12.0-15.0 23.0-26.0 19.0-22.0 22.5-24.5 18.0-21.0 21.0-23.0 26.5-27.8
    Al 4.0-6.0 4.5-6.5 5.0-7.0 4.2-5.0 3.0-4.2 5.0-7.0 6.0-7.0
    RE opportunus
    quantitas
    opportunus
    quantitas
    opportunus
    quantitas
    opportunus
    quantitas
    opportunus
    quantitas
    opportunus
    quantitas
    opportunus
    quantitas
    Fe Requies Requies Requies Requies Requies Requies Requies
    Nb0.5 Mo1.8-2.2
    Maximum continuum
    temperatura servitii
    elementum (ºC)
    950 1250 1250 1250 1100 1350 1400
    Resistivitas
    μΩ.m, 20ºC
    1.25 1.42 1.42 1.35 1.23 1.45 1.53
    Densitas
    (g/cm³)
    7.4 7.10 7.16 7.25 7.35 7.10 7.10
    Thermalis
    conductivitas
    KJ/mhºC
    52.7 46.1 63.2 60.2 46.9 46.1 45.2
    Coefficiens
    expansio linearum
    α×10⁻⁶/ºC
    15.4 16.0 14.7 15.0 13.5 16.0 16.0
    Punctum fusionis °C 1450 1500 1500 1500 1500 MDX MDXX
    Robur tensile
    MPA
    580-680 630-780 630-780 630-780 DC-DCCL 650-800 680-830
    Elongatio apud
    ruptura %
    >16 >12 >12 >12 >12 >12 >10
    Variatio
    area %
    65-75 LX-LXXV 65-75 65-75 65-75 65-75 65-75
    Flexio repetita
    frequentia (F/R)
    >5 >5 >5 >5 >5 >5 >5
    Duritia (HB) 200-260 200-260 200-260 200-260 200-260 200-260 200-260
    Micrographicus
    structura
    Ferritum Ferritum Ferritum Ferritum Ferritum Ferritum Ferritum
    Magneticus
    proprietates
    Magneticus Magneticus Magneticus Magneticus Magneticus Magneticus Magneticus

     

    Mixtura fecalisest mixtura altae resistentiae et calefactionis electricae.Mixtura fecalisTemperaturam processus 2192 ad 2282°F attingere potest, quae temperaturae resistentiae OA 2372°F respondet.

    Solet adhiberi in fornacibus electricis, focis vitreis, calefactoribus tuborum quarzosorum, resistoribus, convertoribus catalyticis, elementis calefactionis, et cetera.