Mixtura Fe-Cr-Al cum resistivitate et temperatura serviendi alta quam mixtura NiCr, et etiam pretio minore. Applicationes:
Resistores electrici ferri-chromii-aluminii late ad fabricanda elementa calefactionis electrica in apparatibus domesticis et ignibus industrialibus adhibentur. Inter applicationes principales sunt ferra crassa, machinae ionizantes, calefactores aquae, formae plastificationis, ferra ad soldandum, elementa tubularia metallica obducta, et elementa cartuchos. Contentum Chemicum % Materia mixturae | Compositio chemica% |
C | P | S | Mn | Si | Cr | Ni | Al | Fe | Alii |
maximum (≤) |
1Cr13Al4 | 0.12 | 0.0025 | 0.0025 | 0.7 | ≤1.00 | 12.5-15.0 | - | 3.5-4.5 | Requies | - |
0Cr15Al5 | 0.12 | 0.0025 | 0.0025 | 0.7 | ≤1.00 | 14.5-15.5 | - | 4.5-5.3 | Requies | - |
0Cr25Al5 | 0.06 | 0.0025 | 0.0025 | 0.7 | ≤0.60 | 23.0-26.0 | ≤0.60 | 4.5-6.5 | Requies | - |
0Cr23Al5 | 0.06 | 0.0025 | 0.0025 | 0.7 | ≤0.60 | 20.5-23.5 | ≤0.60 | 4.2-5.3 | Requies | - |
0Cr21Al6 | 0.06 | 0.0025 | 0.0025 | 0.7 | ≤1.00 | 19.0-22.0 | ≤0.60 | 5.0-7.0 | Requies | - |
0Cr19Al3 | 0.06 | 0.0025 | 0.0025 | 0.7 | ≤1.00 | 18.0-21.0 | ≤0.60 | 3.0-4.2 | Requies | - |
0Cr21Al6Nb | 0.05 | 0.0025 | 0.0025 | 0.7 | ≤0.60 | 21.0-23.0 | ≤0.60 | 5.0-7.0 | Requies | Numerus numericus addendum 0.5 |
0Cr27Al7Mo2 | 0.05 | 0.0025 | 0.0025 | 0.2 | ≤0.40 | 26.5-27.8 | ≤0.60 | 6.0-7.0 | Requies | |
Gradus | 1Cr13Al4 | TK1 | 0Cr25Al5 | 0Cr20Al6RE | 0Cr23Al5 | 0Cr19Al3 | 0Cr21Al6Nb | 0Cr27Al7Mo2 |
Compositio nominalis% | Cr | 12.0-15.0 | 22.0-26.0 | 23.0-26.0 | 19.0-22.0 | 22.5-24.5 | 18.0-21.0 | 21.0-23.0 | 26.5-27.8 |
Al | 4.0-6.0 | 5.0-7.0 | 4.5-6.5 | 5.0-7.0 | 4.2-5.0 | 3.0-4.2 | 5.0-7.0 | 6.0-7.0 |
Re | opportunus | 0.04-1.0 | opportunus | opportunus | opportunus | opportunus | opportunus | opportunus |
Fe | Bal. | | Bal. | Bal. | Bal. | Bal. | Bal. | Bal. |
| | | | | | | Nb0.5 | Mo1.8-2.2 |
Temperatura maxima operandi (°C) | DCCL | 1400 | 1250 | 1250 | 1250 | 1100 | 1350 | 1400 |
Resistivitas 20℃ (Ω/mm²/m) | 1.25 | 1.48 | 1.42 | 1.40 | 1.35 | 1.23 | 1.45 | 1.53 |
Densitas (g/cm³) | 7.4 | 7.1 | 7.1 | 7.16 | 7.25 | 7.35 | 7.1 | 7.1 |
Conductivitas thermalis ad 20℃, W/(M·K) | 0.49 | 0.49 | 0.46 | 0.48 | 3.46 | 0.49 | 0.49 | 0.49 |
Coefficiens Expansionis Linearis (×10¯⁶/℃) 20-1000℃ | 15.4 | 16 | 16 | 14 | 15 | 13.5 | 16 | 16 |
Punctum Liquefactionis Approximatum (℃) | 1450 | MDXX | 1500 | 1500 | 1500 | 1500 | MDX | MDXX |
Robur tensile (N/mm2) | 580-680 | 680-830 | 630-780 | 630-780 | 630-780 | DC-DCCL | 650-800 | 680-830 |
Elongatio (%) | ›16 | ›10 | ›12 | ›12 | ›12 | ›12 | ›12 | ›10 |
Ratio Contractionis Variationis Sectionis (%) | 65-75 | 65-75 | LX-LXXV | 65-75 | 65-75 | 65-75 | 65-75 | 65-75 |
Frequentia Flexionis Iteratae (F/R) | ›5 | ›5 | ›5 | ›5 | ›5 | ›5 | ›5 | ›5 |
Duritia (HB) | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 |
Structura Micrographica | Ferritum | Ferritum | Ferritum | Ferritum | Ferritum | Ferritum | Ferritum | Ferritum |
Proprietas Magnetica | Magneticus | Magneticus | Magneticus | Magneticus | Magneticus | Magneticus | Magneticus | Magneticus |
Vita Celeris (h/℃) | no | ≥80/1350 | ≥80/1300 | ≥80/1300 | ≥80/1300 | ≥80/1250 | ≥50/1350 | ≥50/1350 |