Cronix 70 ad elementa calefactionis electrica corrosioni resistentia in furnis industrialibus cum atmosphaeris reducentibus adhibetur. Cronix 70 oxidationi in aere valde resistit. Usus in elementis calefactionis MgO obductis, aut applicationibus nitrogenium vel atmosphaeras carburantes utentibus, non commendatur.
Gradus | Ni80Cr20 | Ni70Cr30 | Ni60Cr23 | Ni60Cr15 | Ni35Cr20 | Karma | Evanohm | |
Compositio nominalis% | Ni | Bal | Bal | 58.0-63.0 | 55.0-61.0 | 34.0-37.0 | Bal | Bal |
Cr | 20.0-23.0 | 28.0-31.0 | 21.0-25.0 | 15.0-18.0 | 18.0-21.0 | 19.0-21.5 | 19.0-21.5 | |
Fe | ≤1.0 | ≤1.0 | Bal | Bal | Bal | 2.0-3.0 | – | |
Al1.0-1.7 Ti0.3-0.5 | Al2.7-3.2 Mn0.5-1.5 | Al2.7-3.2 Cu2.0-3.0 Mn0.5-1.5 | ||||||
Temperatura maxima operandi (°C) | 1200 | 1250 | 1150 | 1150 | 1100 | trecenti | quadringenti | |
Resistivitas (Ω/cmf, 20℃) | 1.09 | 1.18 | 1.21 | 1.11 | 1.04 | 1.33 | 1.33 | |
Resistivitas (µΩ/m, 60°F) | DCLV | DCCIV | DCCXXVII | DCCLXVIII | DCXXVI | DCCC | DCCC | |
Densitas (g/cm³) | 8.4 | 8.1 | 8.4 | 8.2 | 7.9 | 8.1 | 8.1 | |
Conductivitas Thermalis (KJ/m·h·℃) | 60.3 | 45.2 | 45.2 | 45.2 | 43.8 | 46.0 | 46.0 | |
Coefficiens Expansionis Linearis (×10¯)620-1000℃ (/℃) | 18.0 | 17.0 | 17.0 | 17.0 | 19.0 | - | - | |
Punctum Liquefactionis (℃) | 1400 | 1380 | 1370 | 1390 | 1390 | 1400 | 1400 | |
Duritia (Hv) | CLXXX | CLXXXV | CLXXXV | CLXXX | CLXXX | CLXXX | CLXXX | |
Robur tensile (N/mm)Duo) | DCCCL | DCCCLXXV | DCCC | DCCCL | DCCCL | DCCLXXX | DCCLXXX | |
Elongatio (%) | ≥20 | ≥20 | ≥20 | ≥20 | ≥20 | 10-20 | 10-20 | |
Structura Micrographica | austenita | austenita | austenita | austenita | austenita | austenita | austenita | |
Proprietas Magnetica | Non | Non | Non | Paululum | Non | Non | Non | |
Vita Celeris (h/℃) | ≥81/1200 | ≥50/1250 | ≥81/1200 | ≥81/1200 | ≥81/1200 | - | - |