Compositio chemica:
Exsecutivus norma | Classificatio numerus | Mixtura numerus | Cu | AI | Fe | Mn | Ni | P | Pb | Si | Sn | Zn | Summa totalis alia elementa |
ISO24373 | Cu5210 | CuSn8P | bal. | - | 0.1 | - | 0.2 | 0.01-0.4 | 0.02 | - | 7.5-8.5 | 0..2 | 0.2 |
GB/T9460 | SCu5210 | CuSn8P | bal. | - | maximum 0.1 | - | maximum 0.2 | 0.01-0.4 | maximum 0.02 | - | 7.5-8.5 | maximum 0.2 | maximum 0.2 |
BS EN14640 | Cu5210 | CuSn9P | bal. | - | 0.1 | - | - | 0.01-0.4 | 0.02 | - | 7.5-8.5 | 0.2 | 0.5 |
AWS A5.7 | C52100 | ERCuSn-C | bal. | 0.01 | 0.10 | - | - | 0.10-0.35 | 0.02 | - | 7.5-8.5 | 0.2 | 0.50 |
Proprietates physicae materiarum:
Densitas | kg/m³ | 8.8 |
Spatium fusionis | °C | 875-1025 |
Conductivitas thermalis | W/mK | 66 |
Conductivitas electrica | Sm/mm² | VI-VIII |
Coefficiens expansionis thermalis | 10-6/K(20-300ºC) | 18.5 |
Valores normales metalli conglutinati:
Elongatio | % | 20 |
Robur tensile | N/mm² | 260 |
Opus impactus virgae incisae | J | 32 |
Durities Brinellensis | HB 2.5/62.5 | 80 |
Applicationes:
Mixtura cupri stannei cum altiore duritia stanni percentuale aucta ad soldaduram superimpositam. Praesertim apta ad soldaduram materiarum cuprearum, ut cuprum, aenae stanneae, praesertim ad iungendas mixturas cupri zinci et chalybis. Idonea ad soldaduram reparationis aenorum fusorum et ad soldaduram in furno. Ad soldaduram multistratam in chalybe, soldadura arcus pulsatilis commendatur. Pro magnis operibus, praecalefactio commendatur.
Conficio:
Diameter: 0.80 – 1.00 – 1.20 – 1.60 - 2.40
Spinae: D100, D200, D300, K300, KS300, BS300
Virgae: 1.20 – 5.0 mm × 350mm – 1000 mm
Electroda praesto sunt.
Plures ornatus ad petitionem.
150 0000 2421