Descriptio
Nickel Alloy Monel K-500, stannum aeternum durabile, quod aluminium et titanium continet, praeclaras corrosionis lineamenta resistentiae Monel 400 componit additis beneficiis auctae virium, obdurationis, eiusque virium usque ad 600°C conservans.
Corrosio resistentiae Monel K-D essentialiter eadem est ac Monel 400, excepto quod in conditione dura Monel K-500 magis suscipit accentus corrosioni crepitantis in aliquibus ambitibus.
Aliquae applicationes typicae nickel mixturae K-D sunt ad sentinarum spicula, impulsores, scapulas medicas et strigiles, monilia olei bene terebra, et alia instrumenta complementi, electronicarum partium, fontium et impedimentorum valvae. Hoc mixtura primario adhibetur in applicationibus marinis et oleis et gasi industrialibus. E contra Monel 400 mobilior est, multos usus in tectis, canalibus et architecturae partibus in pluribus aedificiis institutionalibus, fistulae bullientis aqua calentium pascunt, applicationes marinis (vaginas, alias), HF processum alkylationem, productionem et tractationem HF. acidum, et in expolitione uranii, distillationis, condensationis unitates, et fistulae capitis condensationes in refineriis et industriis petrochemicis, et multis aliis.
Compositio chemica
Gradus | Ni% | Cu% | Al% | Ti% | Fe% | Mn% | S% | C% | Si% |
Monel K500 | Min 63 | 27.0-33.0 | 2.30-3.15 | 0.35-0.85 | Max 2.0 | Max 1.5 | Max 0.01 | Max 0.25 | Max 0.5 |
Specifications
Forma | Standard |
Monel K-D | UNS N05500 |
Bar | ASTM B865 |
Filum | AMS4676 |
Sheet/Plate | ASTM B865 |
Forging | ASTM B564 |
Weld Wire | ERNiCu-7 |
Corporalia Properties(20°C)
Gradus | Densitas | Liquefactio Point | Resistivity electrica | Medium Coefficiens Scelerisque Expansion | Scelerisque Conductivity | Imprimis Caloris |
Monel K500 | 8.55g/cm3 | 1315°C-1350°C | 0.615 μΩ•m | 13.7(100°C) a/10-6°C-1 | 19.4(100°C) λ/(W/m•°C) | 418 J/kg•°C |
Mechanica Properties(20°C Min)
Monel K-D | distrahentes Fortitudo | RP0.2% cede virtus | Prolongatio A5% |
Annealed & Anus | Min. 896 MPa | Min. 586MPa | 30-20 |