| Gradus | Ni% | Cu% | Al% | Ti% | Fe% | Mn% | S% | C% | Si% |
| Monel K500 | Min. 63 | 27.0-33.0 | 2.30-3.15 | 0.35-0.85 | Maximus 2.0 | Maximus 1.5 | Maximus 0.01 | Maximus 0.25 | Maximus 0.5 |
Specificationes
| Forma | Norma |
| Monel K-500 | UNS N05500 |
| Taberna | ASTM B865 |
| Filum | AMS4676 |
| Lamina/Tabula | ASTM B865 |
| Cudendo | ASTM B564 |
| Filum suturae | ERNiCu-7 |
Proprietates Physicae(20°C)
| Gradus | Densitas | Punctum Liquefactionis | Resistivitas Electrica | Coefficiens Medius Expansionis Thermalis | Conductivitas Thermalis | Calor Specificus |
| Monel K500 | 8.55g/cm³ | 1315°C-1350°C | 0.615 μΩ•m | 13.7 (100°C) a/10⁻⁶°C⁻¹ | 19.4 (100°C) λ/(W/m•°C) | 418 J/kg•°C |
Proprietates Mechanicae(Minimum 20°C)
| Monel K-500 | Robur Tensilis | Robur Cedendi RP 0.2% | Elongatio A5% |
| Recoctum et Vetustum | Minimum 896 MPa | Minimum 586MPa | XXX-XX |
150 0000 2421