Contentum Chemicum, %
| Ni | Mn | Fe | Si | Cu | Alia | Directiva ROHS Cd | Directiva ROHS de plumbo | Directiva ROHS de Mercurio | Directiva ROHS Cr |
|---|---|---|---|---|---|---|---|---|---|
| 2.0 | - | - | - | Bal | - | ND | ND | ND | ND |
Proprietates Mechanicae
| Nomen Proprietatis | Valor |
|---|---|
| Temperatura Maxima Continua Servitii | 200℃ |
| Resistivitas ad 20℃ | 0.05±10% ohm mm²/m |
| Densitas | 8.9 g/cm³ |
| Conductivitas Thermalis | <120 |
| Punctum Liquefactionis | 1090℃ |
| Robur tensile, N/mm2 Recoctum, Molle | 140~310 MPa |
| Robur Tensilis, N/mm2 Frigidum Laminatum | 280~620 MPa |
| Elongatio (recoctio) | XXV% (minimum) |
| Elongatio (frigide laminata) | 2% (minimum) |
| EMF contra Cu, μV/ºC (0~100ºC) | -12 |
| Structura Micrographica | austenita |
| Proprietas Magnetica | Non |
Mixtura calefactoria CuNi2 resistentiae humilis late in interruptoribus circuitus tensionis humilis, releis oneris thermalis, aliisque productis electricis tensionis humilis adhibetur. Inter materias praecipuas productorum electricorum tensionis humilis numeratur. Materiae a societate nostra productae habent proprietates bonae constantiae resistentiae et stabilitatis superioris. Omnia genera filorum rotundorum, planorum et laminarum praebere possumus.