1. FM60 Oxford Alloy 60ERNiCu-7TIG glutino virga
ERNiCu-7in multis instrumentis, incluso marinis, salibus, et acida minuendis, resistit; Atque adhiberi potest ad deaurationem super chalybem carbonis, modo lavacrum quiddam ERNi-1 pro primo strato adhibetur. Hoc stannum non est aetas durabilis et cum Monel K-500 coniungitur inferiores vires habet quam metallum basis.
Communia nomina: Oxford Alloy® 60 FM 60 Techalloy 418
Standard: AWS 5.14 Classis ERNiCu-7 / ASME SFA 5.14 Classis ERNiCu-7 ASME II, SFA-5.14 UNS N04060 Werkstoff Nr. 2.4377 ISO SNi4060 Europa NiCu30Mn3Ti
Chemical (%)
C | Si | Mn | S | P | Ni |
≤0.15 | ≤1.25 | ≤4.0 | ≤0.015 | ≤0.02 | 62-69 |
Al | Ti | Fe | Cu | alii | |
≤1.25 | 1.5-3.0 | ≤2.5 | Requiem | <0.5 |
WELDING PARAMETERS
Processus | Diameter | Voltage | Amperage | Gas |
TIG | .035″ (0.9mm) .045″ (1.2mm) 1/16″ (1.6mm) 3/32″ (2.4mm) 1/8″ (3.2mm) | 12-15 13-16 14-18 15-20 15-20 | 60-90 80-110 90-130 120-175 150-220 | Argon 100% Argon 100% Argon 100% Argon |
MIG | .035″ (0.9mm) .045″ (1.2mm) 1/16″ (1.6mm) | 26-29 28-32 29-33 | 150-190 180-220 200-250 | 75% Argon+25% Helium 75% Argon+25% Helium 75% Argon + 25% Helium |
SAW | 3/32″ (2.4mm) 1/8″ (3.2mm) 5/32″ (4.0mm) | 28-30 29-32 30-33 | 275-350 350-450 400-550 | Idoneum fluxum potest esse Idoneum fluxum potest esse Idoneum fluxum potest esse |
MACHINA
distrahentes Fortitudo | 76,5000 PSI | 530 MPA |
cede virtus | 52,500 PSI | 360 MPA |
Prolongatio | 34% |
APPLICATIONS
ERNiCu-7 adhiberi potest ad dissimiles applicationes glutino utentes varias admixtiones aeris nickel-aeris ad nickel 200 et ad admixtionem aeris.
ERNiCu-7 ponitur pro arcu gas-tungsten, arcu gasi-metal, et demerso arcu glutino Monel mixturae 400 et K-500.
ERNiCu-7 late in applicationibus marinis propter bonam repugnantiam ad effectus mordax aquae marinae et potatrici usus est.