Normalis compositionem%
Ni | LXXV ~ 76.5 | Fe | Bal. | Mn | 0,3 ~ 0.6 | Si | 0.15 ~ 0.3 |
Mo | - | Cu | 4.8 ~ 5.2 | Cr | 1.8 ~ 2.2 | ||
C | ≤0.03 | P | ≤0.02 | S | ≤0.02 |
Typical mechanica proprietatibus
CEDITAS | Tensile vires | Elongatio |
MPA | MPA | % |
CMLXXX | MXXX | III ~ L |
Typical physica proprietatibus
Density (G / CM3) | 8,6 |
Electrical resistentibus ad 20ºC (OM * mm2 / m) | 0,55 |
Coefficientem linearibus expansion (20ºC ~ 200ºC) x10-6 / ºC | 10,3 ~ 11.5 |
Saturation Magnetostriction coefficientem ΛΘ / 10-6 | 2.4 |
Curie Point TC / ºC | CD |
Magna proprietatibus Alloys cum princeps permeability in infirma agros | |||||||
1J76 | Initial permeability | Maximum permeability | Coercivity | Saturation magnetica inductione intensionem | |||
Сold, advolvit habena / sheet. Crassitudine, mm | Μ0.8 / (MH / M) | μm / (mh / m) | HC / (A / M) | BS / T | |||
Tago | ≤ | ||||||
0.01 mm | 17,5 | 87.5 | 5,6 | 0,75 | |||
0.19 0.19 mm | 25.0 | 162,5 | 2.4 | ||||
0.2 ~ 0.34 mm | 28.0 | 225,0 | 1.6 | ||||
0,35 ~ 1.0 mm | 30.0 | 250.0 | 1.6 | ||||
1.1 ~ 2.5 mm | 27,5 | 225,0 | 1.6 | ||||
2.6 ~ 3.0 mm | 26.3 | 187,5 | 2.0 | ||||
Frigus instructa filum | |||||||
0,1 mm | 6,3 | 50 | 6,4 | ||||
Sera | |||||||
8-100 mm | 25 | C | 3.2 |
Modus calor curatio 1J76 | |
Annealing Media | Vacuum cum RELICTUM pressura non altior quam 0.1PA, hydrogenii cum ros puncto non altior quam minus XL ºC. |
Et calefactio temperatus et rate | MC ~ 1150ºC |
Tenens tempore | III ~ VI |
Refrigerandum rate | Cum C ºc CC / h refrigerat ad DC ºC, cursim refrigeratum ad 300ºC |