Lamina metallica resistentiae chromii ferro-fecralis 0cr25al5
Gradus | 0Cr25Al5 |
Crassitudo 0.565 | 0.56-5mm |
Latitudo | 6-50mm |
Superficies | acido lotus/clarus/oxidatus |
Pondus | 25-30kg/volutum |
Resistivitas | 1.42±0.07μΩ.m |
Temperatura maxima | 1250℃ |
Densitas | 7.1g/cm³ |
Robur tensile | 750N/mm² |
Elongatio | ≥12% |
Gradus | Temperatura maxima | Resistivitas | Punctum fusionis | Robur tensile | Elongatio |
0Cr21Al4 | 1100℃ | 1.23±0.06μΩ.m | 1500℃ | DCCCL | ≥12 |
0Cr25Al5 | 1250℃ | 1.42±0.07μΩ.m | 1500℃ | DCCCL | ≥12 |
0Cr21Al6Nb | 1350℃ | 1.43±0.07μΩ.m | 1510℃ | DCCCL | ≥12 |
0Cr27Al7Mo2 | 1400℃ | 1.53±0.07μΩ.m | 1520℃ | DCCCL | ≥10 |
KSC | 1350℃ | 1.44±0.05μΩ.m | 1510℃ | DCCCL | ≥16 |
Cr20Ni80 | 1200℃ | 1.09±0.05μΩ.m | 1400℃ | DCCCL | ≥20 |
Cr15Ni60 | 1150℃ | 1.12±0.05μΩ.m | 1390℃ | DCCCL | ≥20 |
Cr20Ni35 | 1100℃ | 1.04±0.05μΩ.m | 1390℃ | DCCCL | ≥20 |
Cr20Ni30 | 1100℃ | 1.04±0.05μΩ.m | 1390℃ | DCCCL | ≥20 |
Gradus | Compositio chemica% | ||||||||
C | P | S | Mn | Si | Cr | Ni | Al | Fe | |
≤ | |||||||||
0Cr21Al4 | 0.12 | 0.025 | 0.025 | 0.7 | ≤1.0 | XVII-XXI | ≤0.6 | 3-4 | aequilibrium |
0Cr25Al5 | 0.06 | 0.025 | 0.02 | 0.5 | ≤0.6 | XXIII-XXVI | ≤0.6 | 4.5-6.5 | aequilibrium |
0Cr21Al6Nb | 0.05 | 0.025 | 0.02 | 0.5 | ≤0.6 | XXI-XXIII | ≤0.6 | 5-7 | aequilibrium |
0Cr27Al7Mo2 | 0.05 | 0.025 | 0.02 | 0.2 | ≤0.4 | 26.5-27.8 | ≤0.6 | VI-VII | aequilibrium |
Cr20Ni80 | 0.08 | 0.02 | 0.015 | 0.6 | 0.75-1.6 | XX-XXIII | aequilibrium | <0.5 | ≤1.0 |
Cr15Ni60 | 0.08 | 0.02 | 0.015 | 0.6 | 0.75-1.6 | XV-XVIII | 55-61 | <0.5 | aequilibrium |
Cr20Ni35 | 0.08 | 0.02 | 0.015 | 1.0 | 1-3 | XVIII-XXI | XXXIV-XXXVII | - | aequilibrium |
Cr20Ni30 | 0.08 | 0.02 | 0.015 | 1.0 | 1-3 | XVIII-XXI | XXX-XXXIV | - | aequilibrium |
150 0000 2421